Transverse cracks in welding are defects characterized by cracks that propagate perpendicular to the direction of the weld joint. These cracks can occur due to various factors such as high welding stresses, improper welding parameters, hydrogen embrittlement, or inadequate material selection. Transverse cracks can compromise the integrity and strength of the weld joint, leading to catastrophic failure if not addressed.

Example: Welding of Steel Pressure Vessels

Let’s consider the welding of steel pressure vessels used in industries such as oil refining or chemical processing. Pressure vessels are critical components designed to contain fluids or gases under pressure, and the quality of their welds is paramount for ensuring safe operation.

Transverse Cracks Weld Defect:

During the welding of steel pressure vessels, transverse cracks can occur if proper welding procedures are not followed or if there are issues with welding parameters, joint fit-up, or material properties. This defect manifests as cracks that propagate perpendicular to the direction of the weld joint, visible upon visual inspection or through non-destructive testing techniques.

Determining Transverse Cracks Weld Defect:

  1. Visual Inspection: Transverse cracks can often be visually identified by examining the surface of the weld bead and surrounding areas. Cracks that extend perpendicular to the weld joint indicate the presence of this defect.
  2. Non-Destructive Testing (NDT): Non-destructive testing techniques, such as radiographic testing (RT), ultrasonic testing (UT), or magnetic particle inspection (MPI), can be employed to detect and evaluate the size, location, and extent of transverse cracks within the weld joint.

Radiographic Process:

In radiographic testing (RT) for transverse crack detection:

  • X-rays or gamma rays are directed through the weld joint onto a film or digital detector.
  • Transverse cracks appear as dark, linear indications perpendicular to the direction of the weld joint in radiographic images, indicating areas of discontinuity or fracture.

Prevention Strategies:

  1. Proper Welding Parameters: Control welding parameters, such as voltage, current, travel speed, and preheat temperature, to optimize heat input and minimize the risk of crack formation. Avoid excessive heat input or rapid cooling rates that can promote crack susceptibility.
  2. Joint Fit-Up: Ensure proper fit-up and alignment of the base metals before welding to minimize residual stresses and prevent crack initiation. Proper joint preparation, including beveling or chamfering, can help promote full penetration and fusion without inducing excessive stress concentrations.
  3. Material Selection: Choose appropriate welding materials and filler metals with suitable mechanical properties and chemical compositions to match the base metal and mitigate the risk of crack formation.
  4. Hydrogen Control: Implement measures to control hydrogen levels during welding, such as using low-hydrogen electrodes, preheating the base metal, or implementing post-weld heat treatment (PWHT), to reduce the susceptibility to hydrogen-induced cracking.

Impact on Weld Quality:

Structural Integrity:

Transverse cracks significantly compromise the structural integrity and load-bearing capacity of the weld joint, increasing the risk of sudden failure under mechanical loads or stress.

Leakage Potential:

Transverse cracks can create potential pathways for fluid or gas leakage, particularly in pressure vessels or pipelines, leading to environmental hazards and economic losses.

Repair and Rework:

Transverse cracks may require extensive repair or rework to restore the integrity of the weld joint, resulting in increased labor costs, production delays, and potential project setbacks.

Conclusion:

Transverse cracks in welding are severe defects that require meticulous attention to welding procedures, welding parameters, joint fit-up, and material selection to prevent. Through thorough inspection and testing, including visual examination and non-destructive testing techniques, welders and inspectors can ensure the reliability, safety, and quality of welded components, such as steel pressure vessels, and mitigate the risk of these defects.

By Md Abu Zaed Khan