What is cap undercut weld defect? how to determine
Cap undercut is a weld defect characterized by the formation of a groove or depression at the toe of the weld bead where it meets the base metal. This defect typically occurs due to improper welding technique, such as excessive heat input or incorrect electrode angle, leading to the melting or removal of base metal […]
What is cap undercut weld defect? how to determine Read Post »